First of all, I answer to this question, please correct the errors, if any.
Only after 20 h of carburizing one surface carbon content corresponding to one carbon dioxide content , 20 h of carburizing ago one surface carbon content corresponding to different carburizing time and different carbon dioxide content.
Data are plotted for low-carbon steel carburized at 925C(1700F) in an atmosphere of endothermic carrier gas enriched with propane. Under these conditions, equilibrium was reached only after 20h of carburizing .
在丙烷为富化剂的吸热式气氛中低碳钢925C(1700F)渗碳绘制的数据。在这些条件下只有经过20小时渗碳后表面含碳量与气氛CO2含量达到平衡。
carbon dioxide content of the atmosphere required to develop specific surface carbon levels at different carburizing times under one set of gas-carburizing conditions. Dashed lines indicate the way to determine alternative combinations of treatment time and carbon dioxide content for a single value of surface carbon content.
在一组气体渗碳条件下 不同的渗碳时间 气氛CO2含量需要制定 明确的表面含碳量。虚线
表示以不同数量组合处理时间和二氧化碳含量,来确定表面含碳量单一值的方法。
|