Designation: A 961 – 04
《Standard Specification for Common Requirements for Steel Flanges, Forged Fittings, Valves, and Parts for Piping Applications 1》
7. Heat Treatment
7.1.4Normalizing —Material shall be uniformly reheated to a temperature above the transformation range, and subsequently, cooled in air at room temperature.
|