xiaoxianglou 发表于 2014-3-12 11:53:40

寻找美标ASTM E 384-10?

寻找美标ASTM E 384-10?哪位有这份美标?和国标有什么差异么?

独品沪茗 发表于 2014-3-12 20:04:11

现在是ASTM E384 11-E1版本了。

独品沪茗 发表于 2014-3-12 20:07:12

独品沪茗 发表于 2014-3-12 20:04 static/image/common/back.gif
现在是ASTM E384 11-E1版本了。

不知道咋贴附件:'( 发不了标准

窦信胜 发表于 2014-3-15 19:17:30

Designation: E384 – 11′1
Standard Test Method for
Knoop and Vickers Hardness of Materials1
This standard is issued under the fixed designation E384; the number immediately following the designation indicates the year of
original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. A
superscript epsilon (′) indicates an editorial change since the last revision or reapproval.
This standard has been approved for use by agencies of the Department of Defense.
′1NOTE—Sections 8.3 and A1.1.4 were editorially corrected in March 2012.
......
(减小论坛数据库,已删除)

窦信胜 发表于 2014-3-15 19:18:41

文件不知道怎么传,就把内容都复制了。你需要可以找我

独品沪茗 发表于 2014-3-16 09:40:43

我有中文版本:lol就是不是特别全

xiaoxianglou 发表于 2014-3-19 09:55:15

独品沪茗 发表于 2014-3-12 20:04 static/image/common/back.gif
现在是ASTM E384 11-E1版本了。

可以把这个版本发上来么?

zhengcj 发表于 2014-3-21 15:27:40

独品沪茗 发表于 2014-3-12 20:07 static/image/common/back.gif
不知道咋贴附件 发不了标准

直接在《国外标准》板块发帖即可。
页: [1]
查看完整版本: 寻找美标ASTM E 384-10?