70Mn
谁知道70Mn这种材料,他的化学成分,还有他的热处理曲线???/谢谢了 牌号化学成分(质量分数),%
C(碳)
Si(硅)
Mn(锰)
P(磷)
S(磷)
Cr(铬)
Ni(镍)
15Mn
0.12~0.19
0.17~0.37
0.70~1.00
≤0.035
≤0.035
≤0.25
≤0.25
20Mn
0.17~0.24
0.17~0.37
0.70~1.00
≤0.035
≤0.035
≤0.25
≤0.25
25Mn
0.22~0.30
0.17~0.37
0.70~1.00
≤0.035
≤0.035
≤0.25
≤0.25
30Mn
0.27~0.35
0.17~0.37
0.70~1.00
≤0.035
≤0.035
≤0.25
≤0.25
35Mn
0.32~0.40
0.17~0.37
0.70~1.00
≤0.035
≤0.035
≤0.25
≤0.25
40Mn
0.37~0.45
0.17~0.37
0.70~1.00
≤0.035
≤0.035
≤0.25
≤0.25
45Mn
0.42~0.50
0.17~0.37
0.70~1.00
≤0.035
≤0.035
≤0.25
≤0.25
50Mn
0.48~0.56
0.17~0.37
0.70~1.00
≤0.035
≤0.035
≤0.25
≤0.25
60Mn
0.57~0.65
0.17~0.37
0.70~1.00
≤0.035
≤0.035
≤0.25
≤0.25
65Mn
0.62~0.70
0.17~0.37
0.90~1.20
≤0.035
≤0.035
≤0.25
≤0.25
70Mn
0.67~0.75
0.17~0.37
0.90~1.20
≤0.035
≤0.035
≤0.25
≤0.25
热处理曲线一般要根据自己技术要求制定