Swiss Steel International THYROPLAST? 2083 Plastic Mold Steel
Categories:Metal; Ferrous Metal; Tool Steel; Mold Steel

Material Notes:To manufacture plastic parts, it is necessary to have steels with a high wear resistance, good polishability and etching ability, adequate corrosion resistance, and cost efficient machining properties. Employed for this purpose, as a function of the requirements are case hardening steels, quenched and tempered steels, corrosion-resistant steels, nitriding steels and maraging steels.
Corrosion resistant, good polishability. We recommend the use of vacuum-related THYROPLAST 2083 for the highest demands on polishability.

Applications

molds for processing plastics with corrosive action
Iron content calculated as remainder

Key Words:1.2083, AISI 420
Vendors:No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version   Download as PDFDownload to Excel (requires Excel and Windows)
Export data to your CAD/FEA programAdd to Folder:   My Folder   


Mechanical Properties Metric English Comments
Hardness, Brinell <= 230 <= 230 After soft annealing
Hardness, Rockwell C 40.0 40.0 After tempering at 600°C
51.0 51.0HRC            After tempering at 400°C (回火温度)
52.0 52.0    HRC          After tempering at 500°C (回火温度)
52.0 52.0    HRC         After tempering at 300°C (回火温度)
55.0 55.0    HRC         After tempering at 200°C (回火温度)
56.0 56.0    HRC               after quenching (淬火后)
56.0 56.0   HRC            After tempering at 100°C

Processing Properties Metric English Comments
Annealing Temperature 760 - 800 °C 1400 - 1470 °F Soft Annealing
(退火温度760-800)

化学成分:
Material Components Properties Metric English Comments
Carbon,    C   0.420 % 0.420 %
Chromium,   Cr 13.0 % 13.0 %
Iron,      Fe 86.58 % 86.58 %

redname 发表于 2008-9-18 15:05:47

虽然不是很全,但是还是要谢谢你!

有容乃大 发表于 2008-10-18 11:22:07

原帖由 ych 于 2008-9-17 14:27 发表 http://www.rclbbs.com/images/common/back.gif
2083是瑞士的一种不锈钢,用于注塑模具,如果你懂英文,可以到
www.matweb.com 查看。
Swiss Steel International THYROPLAST? 2083 Plastic Mold Steel
Categories:Metal; Ferrous Metal; Tool Steel; Mold Steel

...
2083好像是德国牌号吧?
页: [1]
查看完整版本: 急求2083的机械性能和相关资料!