盐浴铁素体氮碳共渗的工艺控制

【文章名称】:盐浴铁素体氮碳共渗的工艺控制
【发表期刊】:《热处理》2008年第23卷第1期
【作者】:周鼎华 无锡法福表面处理技术有限公司,江苏无锡214145
【摘要】:全面介绍了一种新的金属表面改性技术,即盐浴铁素体氮碳共渗的工艺过程及其控制要点,渗氮温度和渗氮时间等工艺参数的确定,盐浴中CNO^-和CN^-含量的控制,盐浴的维护,工件的预先热处理以及渗氮质量的检验,并结合生产实际作了说明。
【关键词】:盐浴铁素体氮碳共渗 QPQ 工艺控制

中图分类号:TG156.8+2
文献标识码:B 文章编号:1008-1690(2008)01-0054-004
Process Control of Salt Bath Ferritic Nitrocarburizing


ZHOU Ding-hua
(Wuxi Fafu Techniques Surfaces Treatment Co., Ltd, Wuxi Jiangsu 214145,China)
Abstract: In relation to salt bath ferritic nitrocarburizing, a new surface modification
technology, such problems as technological processes and their control, determination of nitrocarburizing temperature and duration and other parameters, control of CNO and CN contents in the salt bath, maintenance of the salt bath, conditioning heat treatment for workpieces and examination of nitrocarburizing quality, were all-sidedly described. In addition, the salt bath ferritic nitrocarburizing was explained in association with actual production.
Key words:
Salt bath ferritic nitrocarburizing; QPQ; Process control