HEAT TREATMENT Principles and Techniques.Second Edition.2011

《HEAT TREATMENT: Principles and Techniques, Second Edition》T.V. Rajan等.2011
《热处理的原理和工艺》第2版
作者:T. V. Rajan,Ashok Sharma, C. P.
Sharma PHI Learning Private Limited 2011年出版

英文目录:
1. Introduction
2. Nature of Metals and Alloys
3. Iron-Cementite Phase Diagram
4. Principles of Heat Treatment of Steels
5. Heat Treatment Processes for Steels
6. Hardenability
7. Quenchants
8. Chemical Heat Treatment of Steels
9. Surface Hardening
10. Thermomechanical Treatment
11. Heat Treatment Furnaces and Atmosphere
12. Temperature Measurement and Control
13. Possible Defects, Causes and Remedies in Heat Treatment
14. Heat Treatment of Commercial Steels
15. Cast Irons and Their Heat Treatment
16. Heat Treatment of Non-ferrous Metals and Alloys
17. Inspection and Quality Control in Heat Treatment
18. Materials Testing
19. Energy Economy in Heat Treatment

中文目录(人工翻译)
1.概述
2.金属和合金的性质
3.铁碳相图
4.钢的热处理原理
5.钢的热处理工艺
6.淬透性
7.淬火介质
8.钢的化学热处理
9.表面硬化
10.形变热处理
11.热处理炉和气氛
12.温度测量与控制
13.热处理中可能存在的缺陷、原因及补救措施
14.商品钢的热处理
15.铸铁及其热处理
16.有色金属及合金的热处理
17.热处理中的检验与质量控制
18.材料试验
19.热处理的节能

详细目录:





共405页
页: [1]