哪里能够按照DIN 50602:1985 测试非金属夹杂含量
Size: OD 50mm BarMaterial Mark: H13(ESR)
Requirements:
DIN 50602-K1
and the following provisions:
1, test result should be issued in accrodance with table 8 of DIN 50602;
2, the quanity of specimens should be 6, the area of each specimen for evaluation should be not less than 300mm2;
3, the specimens after testing should return.
please furnish the offer informtion, including test total price, test duration. 上海材料研究所
首钢研究所
兴澄钢厂
上钢五厂
东北特钢
等
上述单位或许可以
页: