panpandada
发表于 2009-12-24 16:34:08
是“校直”吧
watereast
发表于 2010-3-16 09:30:42
百分百是矫直,控制椭圆度和长度方向变形的工序
hekailove000
发表于 2010-4-8 15:34:25
应该是straightening
Diego001
发表于 2010-5-8 15:32:58
Most of there pieces are in long parts ,After Heat treatment it shape will change and can not conform the requirement
microsoft
发表于 2010-5-25 15:47:03
轴类零件应该翻译成矫直,套圈类翻译成整形!