电镀常用名词术语英汉对照
化学腐蚀Chemical corrosion双电层Electric double layer
双极性电极Bipolar electrode
分散能力Throwing power
分解电压Decomposition voltage
不溶性阳极(惰性阳极)Inert anode
电化学Electrochemistry
电化学极化(活化极化)Activation polarization
电化学腐蚀Electrochemical corrosion
电化当量Electrochemical equivalent
电导率(比电导)Conductivity
电泳Electrophoresis
电动势Electromotive force
电流密度Current density
电流密度范围Current density range
电流效率Current efficiency
电极Electrode
电极电位Electrode potential
电解质Electrolyte
电解液Electrolytic solution
电离度Degree of ionization
半电池Half-Cell
去极化Depolarization
平衡电极电位Equilibrium electrode-potential
正极Positive electrode
负极Negative electrode
阴极Cathode
阴极极化Cathode polarization
阴极镀层Cathodic coating
阳极Anode
阳极泥Anode slime
阳极极化Anode polarization
阳极镀层Anode coating
迁移数Transport number
过电位Overpotential
扩散层Diffusion layer
杂散电流Stray current
导电盐Conducting salt
光亮电流密度范围Bright current density range
体积电流密度Volume current density
沉积速度Deposition rate
初次电流分布Primary current distribution
局部腐蚀Local corrosion
极化Polarization
极化度Polarizability
极化曲线Polarization curve
极间距Interelectrode distance
乳化Emulsification
应力腐蚀Stress corrosion
析气Gassing
活化Activation
活度Activity
标准电极电位Standard electrode potential
浓差极化Concentration polarization
钝化Passivation
点腐蚀Spot corrosion
络合物Complex compound
复盐Double salt
氢脆Hydrogen embrittlement
界面张力Interfacial tension
临界电流密度Critical current density
原电池(自发电池)Galvanic cell
盐桥Salt bridge
pH值pH Value
基体材料Basis material
辅助阳极Auxiliary anode
辅助阴极Auxiliary cathode
接触电位Contact potential
晶间腐蚀Intercrystauine corrosion
溶度积Solubility product
溶解度Solubility
微观分散能力Microthrowing power
槽电压Tank voltage
静态电极电位Static electrode potential
螯合物Chelate compound
整平作用Leveling action
覆盖能力Covering power
二、镀覆方法
气相沉积Vapor deposition
化学镀Electroless plating
化学钝化Chemical passivation
化学氧化Chemical oxidation
闪镀Flash
电化学氧化(阳极氧化)Anodizing
电镀Electroplating
电铸Electroforming
叠加电流电镀Superimposed current-electroplating
光亮电镀Bright plating
合金电镀Alloy plating
多层电镀Multilayer plating
冲击电流Striking current
金属电沉积Metal electrodeposition
金属喷镀Metal spraying
刷镀Brush plating
周期换向镀Periodic reverse plating
转化膜Conversion coating
挂镀Rack plating
复合电镀(弥散电镀)Composite plating
脉冲电镀Pulse plating
钢铁发蓝(钢铁化学氧化)Blueing
真空镀(真空蒸发镀)Vacuum deposition
热浸镀Hot dipping
离子镀Ion plating
浸镀Immersion plating
高速电镀High Speed electrodeposition
滚镀Barrel plating
塑料电镀Plating on plastics
磷化Phosphating
三、镀前处理、镀后处理和电镀材料
化学抛光Chemical polishing
化学除油Alkaline degreasing
电抛光Electropolshing
电解除油Electrolytic degreasing
电解侵蚀Electrolytic pickling
出光Bright dipping
机械抛光Mechanical polishing
有机溶剂除油Solvent degreasing
光亮侵蚀Bright pickling
汞齐化Blue dip
刷光Brushing
乳化除油Emulsion degreasing
除氢Removal of hydrogen embrittlement
逆流漂洗Countercurrent rinsing
封闭Sealing
染着力Dyeing power
退镀Strip
热扩散Diffusion
热溶Flash melting
预镀Strike
着色Colouring
脱色Decolorization
喷丸Grit blasting
喷砂Sand blasting
喷射清洗Spray rinsing
超声波清洗Ultrasonic cleaning
弱侵蚀Acid dipping
缎面加工Satin finish
强侵蚀Pickling
滚光Barrel burnishing
磨光Grinding
阳极袋Anode bag
光亮剂Brightening agent
助滤剂Filteraid
阻化剂Inhibitor
表面活性剂Surface-active agent
乳化剂Emulsifying agent
络合剂Complexing agent
绝缘层Resist
挂具(夹具)Plating rack
润湿剂Wetting agent
离心干燥机Contrifuger
添加剂Addition agent
缓冲剂Buffer
移动阴极Swept cathode
隔膜Diaphragm
螯合剂Chelating agent
整平剂leveling agent
整流器Rectifier
汇流排Busbar
水的软化Softening of water
大气暴露试验Atmospheric corrosion test
中性盐雾试验Salt spray test
不连续水膜Water breakpH计pH meter
孔隙率Porosity
内应力Internal stress
甘汞电极Calomel electrode
电导仪Conductivity gauge
库仑计(电量计)Coulombmeter
泛点Spotting out
针孔Pores
CASS试验(铜加速盐雾试验)CASS-test
参比电极Reference electrode
变色Tarnish
点滴腐蚀试验Dropping corrosion test
测厚仪Thickness gauge
玻璃电极Glass electrode
结合力Adhesion
哈林槽Haring cell
恒电位法Potentiostatic method
恒电流法Galvanostatic method
树枝状结晶Trees
脆性Embrittlement
起皮Peeling
剥离Spalling
桔皮Orange peel
离子选择性电极Ion selective electrode
海绵状镀层Sponge deposit
烧焦镀层Burnt deposit
麻点Pits
粗糙Stardusting
晶须Whiskers
腐蚀膏试验Corrodkote test
霍尔槽Hull cell 原词:晶间腐蚀Intercrystauine corrosion
更正: 晶间腐蚀Intercrystalline corrosion
页:
[1]