我国热处理的现状及发展方向
我国热处理的现状及发展方向李茂山 赵宝荣 吴光英 张克俭摘 要 从多参数热处理和复合热处理工艺、加热源和加热方式、淬火介质和淬火方法、热处理设备、新材料与热处理工艺相结合、节能和环境保护、热处理生产的自动化和专业化等七个方面,较为全面地论述了我国热处理技术的现状及发展方向。关键词 金属 热加工工艺 热处理 材料工程HEAT-TREATMENT SITUATION AND DEVELOPMENT OF CHINALi Maoshan, Zhao Baorong, Wu Guangying, Zhang KejianABSTRACT This paper summarized the present situation and development direction of heat-treatment of China multiple parament heat-treatment, Composite beat-treatment, heat source, heat type, quenching medium, quenching process, heat-treatment equipment, Combine new material with heat-treatment Process, save energy, environmental protection and automation and speeiality of heat-treatment are mainly introdueed.
KEYWORDS metal, heat techniqne, heat-trentment, material engineering
Correspondent: Li Maoshan, P O Box 4, Baotou 014034