316L环型锻件,如何做冷加工来增加硬度
一批316L环型锻件,外径675MM,内径585MM,高95MM,客户要求硬度达到160HB以上,现在锻件已经粗加工成型,客户自己精加工,
但固溶(1050度)热处理后锻件硬度只有140左右,如何热处理增加硬度 或者 其它办法。
因为客户要精加工,所以提高表面硬度的办法 客户精加工后,所测硬度会降下来。
以下为客户的回复及我的提问,供大家帮我解决问题:
Dear Stephen,
We are going to have hardness requirement for 160HB in future orders. Hence pl. continue your research & development to achieve hardness of minimum 160HB. Our other supplier able to achieve higher hardness by giving higher Chrome & Nitrogen to the max allow as per std.
As per discussion with our Design Dept. I confirm herewith for this particular order we will accept minimum hardness 150HB.
Best Regards,
Vin Talekar
--------------------------------------------------------------------------------
Sent: Tuesday, December 22, 2009 4:24 PM
FOR ITEm 1 of PO IBC350314, the special requirement of HARDNESS is Min. 160HB.
I study the ASTM A182 F316 and VMS-034 REV09 standard,and do not find the requirement for the hardness in the both standards.
As far as i am concerned,for the stainless steel contented low carbon( i.e.F316/F316L/F304) the normal hardness is about 140HB.
It is very difficult to increase the hardness to 160HB by heat-treatment procedure.
The hardness value is 141HB on the test bar.
Tensile Strength=537Mpa
Yield Strength=241Mpa
Elongation=63.6%
Reduction of Area=73%
We try & test heat treatment for test bar several times, but the hardness value can not reach to 160HB.
Please kindly offer your comment!