请教各位前辈老师:昨天收到供应商的机械性能报告,报告中显示断裂后断口处的最小横截面面积Su=0,相应的断面收缩率Z=100%,这应该是不合理的吧?data:image/png;base64,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 是的,断面再小也不会为零,应该是笔误吧 gaoxiuzhe 发表于 2026-4-3 08:31是的,断面再小也不会为零,应该是笔误吧
谢谢:handshake :handshake 这坑定是不合理啊
搞笑了;P闹乌龙呢 这个供应商是外行吧 我想供应商液不会这样要求的,可能是书写笔误,你可以和你们供应商沟通一下。 这样的供应商趁早换掉,发给客户的报告通常有好几道关卡要确认,咋会有这么不靠谱的内容发出来。要么里面的管理制度混乱,要么里面做领导的没有懂技术的.产品质量还能保障啊? 好奇,是什么产品呢,供应商如何测量的?:lol 本帖最后由 后会无期 于 2026-4-7 13:09 编辑
ljjsunny 发表于 2026-4-7 08:41
这样的供应商趁早换掉,发给客户的报告通常有好几道关卡要确认,咋会有这么不靠谱的内容发出来。要么里面的 ...
这是S减速机某工厂找的热处理供应商;P 。我们使用他们的减速机,因为输出轴强度不够,他们进行了热处理,我跟他们要的报告 dchj0532 发表于 2026-4-7 10:56
好奇,是什么产品呢,供应商如何测量的?
减速机的输出轴,因为强度不够,进行了调质 ximenchunxue 发表于 2026-4-7 08:22
我想供应商液不会这样要求的,可能是书写笔误,你可以和你们供应商沟通一下。 ...
问他们了,第一次答复说“就是100%”,又问了一次,还没给回复;P nokin 发表于 2026-4-7 07:23
这个供应商是外行吧
估计不是很专业,我从网上查了一下,是个小厂 MaterialZx 发表于 2026-4-3 10:36
这坑定是不合理啊
同感,所以我挑战了他们;P k克劳德 发表于 2026-4-4 09:33
搞笑了闹乌龙呢
关键是他自己还不清楚这是不合理的:L 后会无期 发表于 2026-4-7 11:08
这是SEW减速机天津工厂找的热处理供应商 。我们使用SEW的减速机,因为输出轴强度不够,他们进行了热处理 ...
下次记得不要把公司名称贴出来!这样不好!!!
难道S某公司都没有机械工程师的吗?收缩率100%,材料是Au吗?但凡这2家公司有个机械专业毕业的也不至于出这样的报告啊? 后会无期 发表于 2026-4-7 11:14
关键是他自己还不清楚这是不合理的
你最好问一下他们检测参考的是什么标准,标准号是什么?检测仪器是否在有效期,检测人员能力是否被确认有效?检测数据有效性的如何保证的?报告出具的流程是什么?岗位职责有没有?
ljjsunny 发表于 2026-4-7 12:22
下次记得不要把公司名称贴出来!这样不好!!!
难道S某公司都没有机械工程师的吗?收缩率100%,材料是Au ...
:handshake 以后注意 可能是软件需要手动输入数值,漏数据结果报告上传了。但是发给客户前居然没人核对也是离谱
本帖最后由 十八街在逃麻花 于 2026-6-16 08:53 编辑
后会无期 发表于 2026-4-7 11:08
这是S减速机某工厂找的热处理供应商 。我们使用他们的减速机,因为输出轴强度不够,他们进行了热处理,我 ...
你应该买的是小型吧,GM的输出轴有相当一部分的材质是C45R,不进炉的,不过断轴八成以上的原因都是客户端负载大或者频繁启停