在翻译一篇外文文章时遇到这个概念,上网搜了一下,知道是与易切削钢有关。。
哪个师傅可以讲一下具体工艺?

Sulfur lowers ductility and toughness in the transverse direction as the content increases. Weldability
decreases with increasing sulfur. Sulfur is very detrimental to surface quality, particularly in the lower
manganese steels. For these reasons, a maximum sulfur content is specified for most steels. However, for
some steels, sulfur is added to improve the machinability. Sulfur also has a pronounced tendency to
segregate. Sulfur occurs in steel primarily in the form of manganese sulfide inclusions. Obviously, greater
frequency of such inclusions is to be expected in the resulfurized grades.

    最后一句中的resulfurize.

签到天数: 69 天

[LV.6]常住居民II

发表于 2008-2-27 19:17:00 | 显示全部楼层
1  再硫化是易切钢的冶炼方法之一,就是回硫的意思。
2  易切钢是国人的叫法,美国佬习惯上叫回硫钢(回硫易切钢)。

[ 本帖最后由 ehai237 于 2008-2-27 19:20 编辑 ]

评分

参与人数 1热处理币 +5 收起 理由
ehai237 + 5 感谢支持!

查看全部评分

回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-11-25 09:30 , Processed in 0.022639 second(s), 22 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表