Hello everybody, i have a question  about calibration accuracy of sensor as below,
According to AMS 2750F table 1,if the calibration accuracy of the type S control sensor is exceed the ±0.6℃ or±0.1%,
shall we scrap the sensor or continue to use the sensor with correction factors?
Hope your answer!

该用户从未签到

发表于 2021-4-9 13:14:18 来自手机 | 显示全部楼层
You shall use the sensor with correction factor. see table1 note(9).
回复 顶 踩

使用道具 举报

签到天数: 96 天

[LV.6]常住居民II

发表于 2021-4-15 09:32:02 | 显示全部楼层
In my opinion, we have to scrap these sensors becuase they can't mee the requirements.

For table 1 Note 9
I think it is only suitable for sensors type not listed in Table 1 and used above 1316℃ then we can follow up the rules of Note 9.
回复 顶 踩

使用道具 举报

签到天数: 21 天

[LV.4]偶尔看看III

发表于 2021-6-21 11:19:43 来自手机 | 显示全部楼层
See table1 note(9).....
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-11-25 09:42 , Processed in 0.024833 second(s), 22 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表