STAINLESS
- stainless steels and their properties
Table of Contents
Introduction .....................................................................................................................................................3
Use of stainless steel ..............................................................................................................................3
How it all started ..................................................................................................................................4
Stainless steel categories and grades..................................................................................................................5
The effects of the alloying elements........................................................................................................5
Corrosion and corrosion properties ...................................................................................................................9
PASSIVITY.............................................................................................................................................9
AQUEOUS CORROSION.........................................................................................................................10
General corrosion.........................................................................................................................10
Pitting and crevice corrosion.........................................................................................................11
Stress corrosion cracking ..............................................................................................................14
Intergranular corrosion..................................................................................................................16
Galvanic corrosion.......................................................................................................................18
HIGH TEMPERATURE CORROSION ..........................................................................................................19
Oxidation.....................................................................................................................................19
Sulphur attack (Sulphidation).......................................................................................................20
Carbon pick-up (Carburization).....................................................................................................21
Nitrogen pick-up (Nitridation).......................................................................................................21
Mechanical properties ....................................................................................................................................23
Room temperature properties...............................................................................................................23
The effect of cold work........................................................................................................................27
Toughness ..........................................................................................................................................27
Fatigue properties ...............................................................................................................................29
High temperature mechanical properties...............................................................................................30
Precipitation and embrittlement .......................................................................................................................32
475°C embrittlement ............................................................................................................................32
Carbide and nitride precipitation ..........................................................................................................32
Intermetallic phases.............................................................................................................................32
Physical properties .........................................................................................................................................34
Property relationships for stainless steels .........................................................................................................36
Martensitic and martensitic-austenitic steels .........................................................................................36
Ferritic steels ......................................................................................................................................36
Ferritic-Austenitic (Duplex) steels........................................................................................................37
Austenitic steels ..................................................................................................................................37
References .....................................................................................................................................................38
Attachment: US, British and European standards on stainless steels..........…………………………41

outokumpu stainless.pdf (463.62 KB, 下载次数: 572)

评分

参与人数 1热处理币 +20 收起 理由
chenze2008 + 20 精品资料!

查看全部评分

签到天数: 131 天

[LV.7]常住居民III

发表于 2010-12-19 18:35:43 | 显示全部楼层
看一下。。。。。
回复 顶 踩

使用道具 举报

该用户从未签到

发表于 2013-2-17 08:53:08 | 显示全部楼层
好东西,收藏了                 
回复 顶 踩

使用道具 举报

签到天数: 5 天

[LV.2]偶尔看看I

发表于 2013-2-18 08:35:30 | 显示全部楼层
好资料,已加分!
回复 顶 踩

使用道具 举报

该用户从未签到

发表于 2013-5-23 16:42:07 | 显示全部楼层
好东西,收藏了,正好有用
回复 顶 踩

使用道具 举报

签到天数: 899 天

[LV.10]以坛为家III

发表于 2013-12-14 02:45:24 | 显示全部楼层
谢谢分享                                                                       
回复 顶 踩

使用道具 举报

该用户从未签到

发表于 2015-11-21 21:36:16 | 显示全部楼层
英文书籍不好找,好的学习材料
回复 顶 踩

使用道具 举报

签到天数: 1254 天

[LV.10]以坛为家III

发表于 2017-12-26 09:35:51 | 显示全部楼层
thanks for sharing . i just want to set up an internal material depot , so this works for me.
回复 顶 踩

使用道具 举报

签到天数: 699 天

[LV.9]以坛为家II

发表于 2021-7-16 09:31:37 | 显示全部楼层
感谢楼主分享~好东西,学习了
回复 顶 踩

使用道具 举报

签到天数: 1237 天

[LV.10]以坛为家III

发表于 2021-7-20 10:05:25 | 显示全部楼层
感谢楼主分享,先顶一下。
回复 顶 踩

使用道具 举报

签到天数: 1023 天

[LV.10]以坛为家III

发表于 2021-9-11 17:37:49 | 显示全部楼层
stainless steels and their properties
回复 顶 踩

使用道具 举报

签到天数: 979 天

[LV.10]以坛为家III

发表于 2023-6-29 09:46:38 | 显示全部楼层
感谢分享好资料,已收藏
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-11-25 09:10 , Processed in 0.028410 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表