[Translation] black body furnace annually

[复制链接]

签到天数: 98 天

[LV.6]常住居民II

发表于 2010-5-25 15:55:46 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
Infrared pyometers shall be calidrated to a black body furnace annually,红外线高温计应使用一个黑体炉每年校准一次。这个黑体炉是什么东西?是翻译成黑体炉吗?

签到天数: 98 天

[LV.6]常住居民II

 楼主| 发表于 2010-5-28 15:16:17 | 显示全部楼层
这么没有人回答
回复 顶 踩

使用道具 举报

签到天数: 80 天

[LV.6]常住居民II

发表于 2010-5-28 16:56:40 | 显示全部楼层
本帖最后由 wty728 于 2010-5-28 17:01 编辑

Blackbody Calibration Source Truths
A precision blackbody (black body) is a controlled source of thermal radiation used to calibrate infrared radiation thermometers (pyrometers), thermal imagers and radiation heat flux gauges and radiometers. They are highly specialized and have been described and developed since Max Planck invented the concept at the end of the 19th century.

Needless to say, a practical blackbody simulates Planck's ideal source and the closeness of that simulation to the ideal, the more expensive they are. So, selection of one is a careful exercise in tradeoffs of needs versus cost. One, of course, must know what they need before selecting a given unit.

Blackbody thermal radiation sources are not something purchased every day, yet they are often kept for years. Some are used infrequently. Some are used with surprising regularity. So, a blackbody purchase is done usually with great care. On the connecting pages and links we have put together a few more helpful truths about them and some key specification components that must be considered.

可到网上查看这份文献资料,估计有帮助
一种便携式中温固定点黑体炉
A Portable Black Body Furnace With Fixed Middle Temperature Points
介绍一种用于固定点准确复现的黑体炉,应用该装置,复现铟、锡和锌点温度的总不确定度为±0.21℃.这种黑体炉可以作为标准装置进行实验室比对以及对红外测温仪进行现场检定.

评分

参与人数 1热处理币 +5 收起 理由
bill_bush + 5 感谢参与!

查看全部评分

回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-11-25 09:20 , Processed in 0.023362 second(s), 22 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表