ASTM A575-96 (R2013) Standard Specification for Steel Bars, Carbon, Merchant ...

[复制链接]

签到天数: 3055 天

[LV.Master]伴坛终老

发表于 2024-5-22 06:39:43 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
ASTM A575-96 (R2013) Standard Specification for Steel Bars, Carbon, Merchant Quality, M-Grades
This standard is issued under the fixed designation A575; the number immediately following the designation indicates the year of
original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. A
superscript epsilon ® indicates an editorial change since the last revision or reapproval.
This standard has been approved for use by agencies of the Department of Defense.

ASTM A575-96 (R2013) Standard Specification for Steel Bars, Carbon, Merchant Qua.pdf (1.03 MB, 下载次数: 17)

签到天数: 1787 天

[LV.Master]伴坛终老

发表于 2024-5-22 08:35:09 | 显示全部楼层
ASTM A575-96 (R2013) 碳钢、商业质量、M 级钢棒的标准规范 该标准以固定名称 A575 发布;紧随名称后的数字表示最初通过的年份,或者在修订的情况下,表示最后修订的年份。括号中的数字表示上次重新批准的年份。上标 epsilon ®表示自上次修订或重新批准以来的编辑更改。该标准已被国防部机构批准使用。
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-11-6 07:23 , Processed in 0.024154 second(s), 24 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表