[Discussion] dew Point testing

[复制链接]

签到天数: 124 天

[LV.7]常住居民III

发表于 2011-4-29 21:19:23 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
法国公司标准
:For parts heat treated in vacuum furnace, the following requirements shall be fulfilled:
(4) Dew point shall be equal or lower than -54 °C (-65 °F).
(5) Dew point shall be measured and recorded continuously. For specific furnaces (eg integral
oil quench furnace) any deviation shall be validated by the Competent Authority.

AMS2769B
3.2 Partial Pressure Atmospheres
Analysis of the dewpoint at the location of replenishment is not required, however, the dew point of the gas
shall be - 60 ºF or lower as the gas enters the furnace and shall be verified at least quarterly .

真空油淬不分压是否需要测N2露点
N2只用于洗炉淬火时隔开加热室与装料室.

签到天数: 35 天

[LV.5]常住居民I

发表于 2011-4-30 01:37:58 | 显示全部楼层
回复 1# 混在西北


    应该是指的炉内气氛露点吧
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-11-25 09:41 , Processed in 0.022531 second(s), 21 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表