北京中仪天信科技有限公司
Designation: A255-10 (Reapproved 2018)
Standard Test Methods for Determining Hardenability of Steel
This standard is issued under the fixed designation A255; the number immediately following the designation indicates the year of original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. A superscript epsilon (´) indicates an editorial change since the last revision or reapproval.
This standard has been approved for use by agencies ofthe U.S. Department ofDefense

ASTM A255-10(2018) Standard Test Methods for Determining Hardenability of Steel.pdf

17.52 MB, 下载次数: 24

售价: 1 枚热处理币  [记录]

您需要登录后才可以回帖 登录 | 免费注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-8-26 09:40 , Processed in 0.024364 second(s), 25 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表