阴极保护作用cathodic protection for all kinds of parts ( fasteners >M6 )•优异的防腐性能•excellent prevention of ground-metal corrosion ( red rust ) bysacrificial galvanic corrosion protectionbarrier-effect of overlapping zinc –and aluminumflakesself healing-effect ( migration of zinc-corrosion-products )•好的耐热性good heat-resistance •耐化学性能好good resistance against oil, gasoline, organic-solvents, brake-fluid