发表于 2007-7-2 12:10:19 | 显示全部楼层 |阅读模式
北京中仪天信科技有限公司
Solution Heat Treatment in a Roller Hearth Furnace

Roller Hearth Solution Heat Treat Furnace & Age Oven

The roller hearth furnace line can be employed to heat treat aluminum castings or forgings on a batch/continuous basis.  The work is loaded on racks or trays for automatic processing through the entire system.  

The furnace is divided into two main zones, one for heating and one for soaking.  As racks are charged, they continually move through the unit at a predetermined speed.  As the racks approach an internal or external door, a photo-eye signals their location and opens the door.  Independently clutched high speed drives then move the racks forward quickly, and stop them automatically at the next position.  When the rack reaches the end of the furnace, the rear door is then opened and the rack is quickly moved onto the quench elevator and lowered into the quench tank.
Depending upon the alloy that is being heat treated, artificial aging may be required to produce the proper hardness qualities.  In castings, hardness can be achieved at ambient conditions if the part remains at rest for a period of time.  This is generally not possible as other finishing steps such as machining or painting must be done to maintain production flow at a normal pace.  To speed up the hardening process, artificial aging is employed.  By raising the temperature of the the work to approximately 350 degrees F, and holding it there for approximately 3-4 hours, hardening will occur.  When aging is finished, further processes such as those mentioned can take place.

For extruded alloys, the soaking time is generally minimal.  In these cases, the work is heated to temperature and stabilized for a short period of time and quenched.  Since extrusions can be in various forms, such as rod, bar, tubing, etc., the furnace many require special considerations that are much different from those mentioned up to this point.  Handling of extrusions at solution heat treating temperatures can pose a new set of problems in designing a furnace.  One example is shown in figure #3 where the work is placed directly on the rolls.  Continuous roll oscillation is used to control distortion of the work.  Since the work length approached 52 inches, quenching of these sections is accomplished "on the fly" as they are discharged out of the furnace.  The quench enclosure contains a series of spray nozzles positioned above and below the rolls which cools the work as it passes through.  The speed at which the work is passing, the volume of water, and the pressure of the spray becomes extremely important.

Determining the exit design depends primarily on the process requirement for the alloy and the work configuration.  Whatever the process requirements, SECO/WARWICK has the equipment for your solution heat treating needs.

rollerhearth.pdf

514.76 KB, 下载次数: 277

评分

参与人数 1热处理币 +20 收起 理由
慕山慕水 + 20 感谢上传!

查看全部评分

该用户从未签到

发表于 2007-9-20 09:48:30 | 显示全部楼层
extruded alloys

评分

参与人数 1热处理币 -3 收起 理由
stove -3 灌水嫌疑!

查看全部评分

回复 顶 踩

使用道具 举报

该用户从未签到

发表于 2011-3-16 16:10:19 | 显示全部楼层
楼主能否给个中文翻译
回复 顶 踩

使用道具 举报

该用户从未签到

发表于 2011-6-11 12:23:08 | 显示全部楼层
不错的资料 谢谢楼主的分享
回复 顶 踩

使用道具 举报

签到天数: 1680 天

[LV.Master]伴坛终老

发表于 2011-7-6 08:15:23 | 显示全部楼层
铝合金的,真空锁气的。。。。
回复 顶 踩

使用道具 举报

签到天数: 1 天

[LV.1]初来乍到

发表于 2012-10-9 20:24:04 | 显示全部楼层
真的看不懂,希望楼主翻译下
回复 顶 踩

使用道具 举报

该用户从未签到

发表于 2012-10-9 20:45:09 | 显示全部楼层
本帖最后由 djh088 于 2012-10-10 08:16 编辑

用英文抬高自己,上国外网站到处都是,这是中文网站,还是讲国语,用国文,干嘛?告诉你,你的英文不太好,不要丢人了,难道你用外文就证明你的热处理水平吗?这种帖子还评分,一伙的,在炒作!
回复 顶 踩

使用道具 举报

您需要登录后才可以回帖 登录 | 立即注册

本版积分规则

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备2021037530号|苏公网安备32059002001695号 )
Copyright © 2005-2026, rclbbs.com 苏州热协网络技术有限公司 版权所有

GMT+8, 2026-11-8 14:42 , Processed in 0.029488 second(s), 30 queries .

Powered by Discuz! X3.5

© 2001-2026 Discuz! Team.

快速回复 返回顶部 返回列表